Effect of finishing/polishing techniques and time on surface roughness of esthetic restorative materials


1 Department of Dental Materials, Manipal College of Dental Sciences, Manipal University, Mangalore, Karnataka, India
2 Department of Conservative Dentistry and Endodontics, Manipal College of Dental Sciences, Manipal University, Mangalore, Karnataka, India
3 Department of Oral Pathology, Manipal College of Dental Sciences, Manipal University, Mangalore, Karnataka, India
4 Dental Materials, Manipal College of Dental Sciences, Mangalore, Manipal University, Mangalore, Karnataka, India

Correspondence Address:
Shreya Hegde
Department of Conservative Dentistry and Endodontics, Manipal College of Dental Sciences, Mangalore, Manipal University, Mangalore, Karnataka
India
Login to access the Email id

Source of Support: None, Conflict of Interest: None


DOI: 10.4103/1735-3327.215962

Rights and Permissions

Background: Surface roughness associated with improper finishing/polishing of restorations can result in plaque accumulation, gingival irritation, surface staining, and poor esthetic of restored teeth. The study aimed to evaluate the efficiency of various finishing and polishing systems and time using various procedures on surface roughness of some esthetic restorative materials. Materials and Methods: In this in vitro study, samples of two composite materials, compomer and glass ionomer cement (GIC) materials, were fabricated. Finishing and polishing were done immediately (n = 40) and after 1 week (n = 40) using four systems (diamond bur + soflex discs; diamond bur + Astropol polishing brush; tungsten carbide bur + soflex discs; tungsten carbide bur + Astropol polishing brush). Surface roughness was measured using surface profilometer. Data were statistically analyzed by t-test (for each material and time period) and one-way analysis of variance followed by Tukey's post hoc (for finishing and polishing systems) at a significant level of P < 0.05. Results: Analysis of time period, irrespective of finishing and polishing system showed that Ra values were greater (P < 0.05) in delayed polishing in GIC > Z100 > Filtek P90 > Dyract AP, suggesting immediate polishing is better. Among the materials, Filtek P90 had the least Ra values indicating the smoothest surface among all materials, followed by Z100, Dyract AP, and GIC. Comparison of polishing and finishing systems irrespective of materials showed that Ra values were lower (P > 0.05) in diamond + Astropol combination whereas diamond + soflex had the greatest Ra values. Conclusion: It might be concluded that: (i) Filtek P90 showed least Ra values followed by < Z100 < Dyract < GIC; (ii) immediate (24 h) finishing/polishing of materials is better than delayed; and (iii) among all these polishing systems, diamond bur–Astropol and Astrobrush showed good surface finish.


[FULL TEXT] [PDF]*
Print this article     Email this article
 Next article
 Previous article
 Table of Contents

 Similar in PUBMED
   Search Pubmed for
   Search in Google Scholar for
 Related articles
 Citation Manager
 Access Statistics
 Reader Comments
 Email Alert *
 Add to My List *
 * Requires registration (Free)
 

 Article Access Statistics
    Viewed143    
    Printed3    
    Emailed0    
    PDF Downloaded39    
    Comments [Add]    

Recommend this journal